Geometry Criterion: Difference between revisions
Oluschinski (talk | contribs) Created page with "{{Language_sel|LANG=ger|ARTIKEL=Geometriekriterium}} {{PSM_Infobox}} <span style="font-size:1.2em;font-weight:bold;">Geometry criterion</span> __FORCETOC__ ==Geometry criterion, fracture tougness== In the linear-elastic approach, the geometric variables ''B'', ''a'' and the ligament expansion (''W''–''a'') are estimated using the empirically determined relationship {| |- |width="20px"| |width="500px" | <math>B{,}\ a{,}\ \left( W-a\right)\,\ge\,\beta \left( \frac{K}{\..." |
(No difference)
|
Latest revision as of 09:39, 2 December 2025
| A service provided by |
|---|
|
| Polymer Service GmbH Merseburg |
| Tel.: +49 3461 30889-50 E-Mail: info@psm-merseburg.de Web: https://www.psm-merseburg.de |
| Our further education offers: https://www.psm-merseburg.de/weiterbildung |
| PSM on Wikipedia: https://de.wikipedia.org/wiki/Polymer Service Merseburg |
Geometry criterion
Geometry criterion, fracture tougness
In the linear-elastic approach, the geometric variables B, a and the ligament expansion (W–a) are estimated using the empirically determined relationship
with
| y | Yield stress (yield point). |
The geometry constant is material-dependent.
Experimental results regarding the influence of the test specimen thickness B on the fracture mechanical properties (see: fracture mechanical testing) for plastics are available in the literature. Figure 1 shows the dependence of the coefficient according to the above equation on the fracture toughness determined under quasi-static and impact loading (see: impact loading of plastics) for various plastics. The relationship shown was established on the basis of experimentally determined thickness and a/W dependencies and has a high degree of generalisation, as a common relationship results regardless of the type of stress (quasi-static, impact) and the material failure (stable, unstable) (see: Crack propagation).
| Fig. 1: | Dependence of the coefficient on the fracture toughness KIc, KId for different plastics |
References
- Blumenauer, H., Pusch, G.: Technische Bruchmechanik. Deutscher Verlag für Grundstoffindustrie, Leipzig Stuttgart (1993) (ISBN 3-342-00659-5; see AMK-Library under E 29-3)
- Anderson, T. L.: Fracture Mechanics. Fundamentals and Applications. 3rd Ed., CRC Press, Boca Raton (2005) (ISBN 978-0849342608; see AMK-Library under E 8-2), DOI: https://doi.org/10.1201/9781315370293
- Grellmann, W., Seidler, S., Lach, R.: Geometrieunabhängige bruchmechanische Werkstoffkenngrößen – Voraussetzung für die Zähigkeitscharakterisierung von Kunststoffen. Materialwissenschaften und Werkstofftechnik 32 (2001) 552–561, https://doi.org/10.1002/1521-4052(200106)32:6%3C552::AID-MAWE552%3E3.0.CO;2-O
- Akay, M.: Fracture Mechanics Properties. In: Brown, R. P. (Ed.): Handbook of Polymer Testing. Marcel Dekker Inc., New York (1999) 533–588 (ISBN 978-0824701710; see AMK-Library under C 5)
Geometry criterion, J-integral concept
Due to the elastic-plastic material behaviour typical of plastics, especially with decreasing test specimen thickness, decreasing stress velocity and increasing temperature, and the limits for the applicability of linear-elastic fracture mechanics, it is necessary to use the J-integral concept to describe the geometry dependence. The critical J-values are geometry-independent if the criterion
with
| material-dependent constant of the geometry criterion of the J-integral concept |
is fulfilled.
For the geometry constant from this criterion, Figure 2 shows a tendency to decrease with increasing toughness, which , like the geometry constant , must be regarded as a material-dependent variable and can assume values between 5 and 1220, which represent maximum values for impact loading.
| Fig. 2: | Dependence of the coefficients on the J-value for different plastics |
Knowledge of the general -J relationship allows the required test specimen thicknesses to be estimated. The advantage of determining fracture mechanics values under impact loading lies in the possibility of obtaining geometry-independent values even at low test specimen thicknesses.
References
- Grellmann, W., Seidler, S., Lach, R.: Geometrieunabhängige bruchmechanische Werkstoffkenngrößen – Voraussetzung für die Zähigkeitscharakterisierung von Kunststoffen. Materialwissenschaften und Werkstofftechnik 32 (2001) 552–561
- Grellmann, W.: New Developments in Toughness Evaluation of Polymers and Compounds by Fracture Mechanics. In: Grellmann, W., Seidler, S.: Deformation and Fracture Behaviour of Polymers. Springer Berlin Heidelberg (2001) p. 3–26, (ISBN 3-540-41247-6; see AMK-Library under A 7)
Geometry criterion, crack opening displacement
The requirements for the test specimen geometry are estimated using the Crack tip opening displacement concept
| . |
with
| material-dependent constant of the geometry criterion of the CTOD concept |
| Fig. 3: | Dependence of the coefficient on the critical crack opening Idk |
In addition to the J-integral concept, the CTOD concept is used in particular to describe deformation-determined fracture processes. The prerequisite for determining critical crack openings is the formation of a quasi-static stress state. On the basis of the “Plastic Hinge Model”, the critical crack opening is determined for impact-type loading, which is independent of the a/W ratio at B = 4 mm for a/W > 0.2. Figure 3 shows that -values between 10 and 90 can be assumed and that a considerable overestimation of the required minimum test specimen dimensions is possible if the necessary notch depth or test specimen thickness is still unknown.
See also
References
- Grellmann, W., Seidler, S.: Determination of Geometry Independent Fracture Mechanics Values of Polymers. Int. J. of Fracture 68 (1994) R19–R22, https://doi.org/10.1007/BF00032333
- Grellmann, W., Seidler, S., Hesse, W.: Procedure for Determining the Crack Resistance Behaviour Using the Instrumented Charpy Impact Test. In: Grellmann, W., Seidler, S.: Deformation and Fracture Behaviour of Polymers. Springer Berlin Heidelberg (2001) S. 71–86, (ISBN 3-540-41247-6; AMK-Library under A 7)